LBT Faceplate Remelting Images -- June 1997

c
a
m
e
r
a
New glass loaded onto the LBT mirror.

09 June 22:55 UT
Melting glass inside the oven.

11 June 01:42 UT
Maximum temperature of 1180 degrees C.

11 June 06:37 UT
Faceplate seen during the cooling process.

13 June 06:46 UT
A
B
D
E

The full-size JPEG images linked above are typically 65 - 92 Kbytes in size.

To the previous page

by: Anna Rosa Lampis, Yuliya Shlemenzon and J. M. Hill

Last modified: Sat Jun 14 13:18:19 1997